Choose the size
- Ø 0.8 mm · K300 15–20 kg≈ 15 kg
- Ø 1 mm · K300 15–20 kg≈ 15 kg
- Ø 1.2 mm · K300 15–20 kg≈ 15 kg
- Ø 1.6 mm · K300 15–20 kg≈ 15 kg
Indicative diameters; confirmed with the order
Supply programme: spools on request D100 (0.5–1 kg), D200 (2–5 kg)
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
4.71–6.79 kg
of DT-1.4576 MIG for 10 m of weld
1 pack of ≈ 15 kg
Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
For joining and surfacing on stabilised, similar, corrosion-resisting CrNiMo steels for severely corrosive service, at service temperatures up to 400 °C.
Base metals
1.44011.44041.45711.45731.45801.45811.4583
| Polarity | DC+ |
|---|---|
| Shielding gas | M11, M12, M13 |
Classification and approvals
Classification
| AWS class | ER 318 Si |
|---|---|
| EN ISO class | G 19 12 3 Nb Si |
| Material no. (W.-Nr.) | 1.4576 |
| ISO 14343-B | SS318Si |
Approvals
- TÜV, DB, CE
According to the Dratec 2025 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the wire
| C | 0.06 |
|---|---|
| Cr | 19.0 |
| Mn | 1.50 |
| Mo | 2.60 |
| Nb | 12×C |
| Ni | 12.0 |
| Si | 0.85 |
Values in mass %.
Mechanical properties
guide values
| Yield strength (Rp0.2) | 510 MPa |
|---|---|
| Tensile strength (Rm) | 650 MPa |
| Elongation (A5) | 30 % |
| Impact energy (KV) | 65 J |
| Service temperature | −120–400 °C |
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Rm | KV | Availability |
|---|---|---|---|---|
| ELOX SG 318 Si MIGGedik | G 19 12 3 Nb Si | 600–780 MPa | min. 63 J (20 °C) | To order · price and lead time in the quote |